Polymer Property : Tensile Strength = 62.1 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 48.3 - 62.1 MPa
7000 - 9000 psi
ASTM D638
Mar-Bal MB1000-15 Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
Tensile Strength 41.4 - 62.1 MPa
6000 - 9000 psi
ASTM D638
Mar-Bal MB3000-20NY Thermoset Polyester Composite Molding Compound
A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc.
Tensile Strength 48.3 - 62.1 MPa
7000 - 9000 psi
Bulk Molding Compounds BMC 6241 Glass Reinforced BMC
BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availab..
Tensile Strength 48.3 - 62.1 MPa
7000 - 9000 psi
Bulk Molding Compounds BMC T9 General Purpose Molding Compound
BMC T9 is a low cost, general purpose bulk molding compound designed for the electrical industry. It is UL listed and is used extensively in the manufacture of residential circuit breakers. BMC T9..
Tensile Strength 48.3 - 62.1 MPa
7000 - 9000 psi
Bulk Molding Compounds BMC T12-15526 General Purpose Molding Compound
BMC T12-15526 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. ..
Tensile Strength 48.3 - 62.1 MPa
7000 - 9000 psi
Bulk Molding Compounds BMC T12-15541 General Purpose Molding Compound
BMC T12 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Typica..