Mechanical Properties Metric English Comments
Tensile Strength 58.0 MPa
8410 psi
ASTM D638
Premix Premi-Glas® 2550® AM CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas 2550® AM CR-SX is an advanced fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications where stringent flame spread and smoke generati..
Tensile Strength 58.0 MPa
8410 psi
ASTM D638
Premix Premi-Glas® 2550® CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas 2550® CR-SX is an advanced fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications where stringent flame spread and smoke generation ..
Tensile Strength 58.0 MPa
8410 psi
ASTM D638
Kolon KOCETAL® DS500 Acid Resistant Acetal Resin
Improved acid resistance. Applications: Products for improved chemical resistance. Information provided by API-Kolon.
Tensile Strength 58.0 MPa
8410 psi
ASTM D638
Kolon KOCETAL® LW701 Wear Modified Acetal Resin
Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon.
Tensile Strength 58.0 MPa
8410 psi
ASTM D638
Kolon SPESIN® KP515FLBL High Impact PBT Alloy Resin
High elastic, whether resistantApplications: WipersInformation provided by API-Kolon.
Tensile Strength 58.0 MPa
8410 psi
ISO 527
Lucite International Diakon® ST25G7 Toughened Acrylic Compound
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by..
Tensile Strength 58.0 MPa
8410 psi
ISO 527
Lucite International Diakon® TD525 Toughened Acrylic Compound
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by..
Tensile Strength 58.0 MPa
8410 psi
dry; ISO 527
Ter Hell Plastic Terez® 3610/4 PA/ABS Blend
Impact resistant blend with reduced moisture absorption and good flowability.Application: For molding parts with increased demand of impact strength and cold impact strength. For injection molding..
Tensile Strength 58.0 MPa

@Strain 15.0 %,
Temperature 23.0 °C
8410 psi

@Strain 15.0 %,
Temperature 73.4 °F
50 mm/min; ISO 527-2
BASF Elastollan R 1000 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Tensile Strength 58.0 MPa
8410 psi
ISO 527
Premix Thermoplastics PRE-ELEC® PA 1409 Conductive Thermoplastic Compound
PRE-ELEC® PA 1409 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1..
Tensile Strength 58.0 MPa
8410 psi
ISO 527-1
Sax Polymers SAXATEC 4210 Acrylonitrile Styrene Acrylate
SAXATEC 4210 is a high heat resistant, high viscosity and weatherable ASA injection molding grade, characterized by high impact strength and high stiffness.Information provided by SAX Polymers