Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 55.0 MPa | 7980 psi | ASTM D638 |
Premix Premi-Glas® 1200-22 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-22 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Tensile Strength | 55.0 MPa | 7980 psi | ASTM D638 |
Premix Premi-Glas® 1200H-22 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-22 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go.. |
|||
Tensile Strength | 55.0 MPa | 7980 psi | ASTM D638 |
Premix Premi-Glas® 2200-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Tensile Strength | 55.0 MPa | 7980 psi | ASTM D638 |
Premix Premi-Glas® 2203-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Tensile Strength | 55.0 MPa | 7980 psi | ASTM D638 |
Premix Premi-Glas® 2203-22 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-22 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Tensile Strength | 55.0 MPa | 7980 psi | ASTM D638 |
Premix Premi-Glas® 2204-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Tensile Strength | 55.0 MPa | 7980 psi | ASTM D638 |
Premix Premi-Glas® 2205-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Tensile Strength | 55.0 MPa | 7980 psi | ISO 527 |
Premix Thermoplastics PREBOARD E1026 Standard Epoxy Circuit Boards PREBOARD is a thermoplastic based PCB laminate. Low dissipation factor leads to high gain in the antennas. As a non filled laminate PREBOARD is fully homogenous so that consistant properties are ac.. |
|||
Tensile Strength | 55.0 MPa | 7980 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® PA 1412 Conductive Thermoplastic Compound PRE-ELEC® PA 1412 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1.. |
|||
Tensile Strength | 55.0 MPa | 7980 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP Ertacetal® H-TF POM-H, PTFE-filled, extruded (ISO Data) Ertacetal H-TF is a DELRIN® AF Blend, a combination of TEFLON® fibres evenly dispersed in a DELRIN acetal resin. Much of the strength that is inherent in Ertacetal H is retained. Some properties c.. |
|||
Tensile Strength | 55.0 MPa | 7980 psi | ISO 527-2 |
NOVA Chemicals Dylark® 520XT Glass Reinforced Engineering Resin Features: Higher toughness product, Excellent stiffness, High heat resistance, Superior adhesion to urethane foamApplications: Instrument panel substrates, Mid-Consoles, Center Stacks, Interior tri.. |
|||
Tensile Strength | 55.0 MPa | 7980 psi | ASTM D638 |
Kolon KOCETAL® CB301 Conductive Grade Acetal Resin Conductive grade. Applications: Conductive products. Information provided by API-Kolon. |
|||
Tensile Strength | 55.0 MPa | 7980 psi | |
Lucite International Lucite® 41 Acrylic Resin for Casting and Embedments Lucite® 41 is a high molecular weight methyl methacrylate homopolymer for use in castings & embedments.Like all Lucite® Acrylic Resins for castings & embedments, Lucite® 41 offers: Exceptio.. |
|||
Tensile Strength | 55.0 MPa | 7980 psi | ISO 527-1 |
Sax Polymers SAXLAC 207 Acrylonitrile Butadiene Styrene Saxalac 207 is a high heat ABS, characterized by high impact strength and high stiffness.Mechanical property data tested at 50% RH.Information provided by SAX Polymers |
|||
Tensile Strength | 55.0 MPa | 7980 psi | dry; ISO 527 |
Ter Hell Plastic Terez® PA 6 7450 T GK 30 Polyamide 6, 30% Glass Fiber Description: Polyamide 6 medium viscosity, heat impact resistant and 30% glass bead reinforced.Application: For low warpage molding parts with balanced shrinkage characteristics.Information provide.. |
|||
Tensile Strength | 55.0 MPa | 7980 psi | ISO 37 |
BASF Elastollan B 60 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 55.0 MPa | 7980 psi | ISO 37 |
BASF Elastollan B 64 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 55.0 MPa | 7980 psi | ISO 37 |
BASF Elastollan B 90 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | >= 55.0 MPa | >= 7980 psi | ISO 37 |
Austin Novel Materials Texalan® 272D Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tensile Strength | 55.0 MPa | 7980 psi | ISO 37 |
BASF Elastollan B 85 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 55.0 MPa @Strain 5.00 %, Temperature 23.0 °C |
7980 psi @Strain 5.00 %, Temperature 73.4 °F |
50 mm/min; ISO 527-2 |
BASF Elastollan R 2000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Tensile Strength | 55.0 MPa | 7980 psi | ISO 37 |
BASF Elastollan S 85 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 55.0 MPa | 7980 psi | ISO 37 |
BASF Elastollan S 90 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 55.0 MPa | 7980 psi | |
Perstorp Compounds Akestra™ 100 Thermoplastic Copolyester Excellent appearance, clarity, hydrolytic stability, heat resistance and high strength. Used for extrusion and injection molded articles, blow molding, films and sheets. It can be used as a polyst.. |
|||
Tensile Strength | 55.0 MPa | 7980 psi | DIN 53 455 |
Hippe PVDF Better mechanical strength compared to other fluorinated polymers. Tough and hard. High-grade electrical feature. Good weathering stability. Physiologically safe. Not as good as fluorinated pol.. |
|||
Tensile Strength | >= 55.0 MPa | >= 7980 psi | ISO 37 |
Austin Novel Materials Texalan® 572D Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Tensile Strength | 55.0 MPa | 7980 psi | ISO 37 |
BASF Elastollan B 95 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 55.0 MPa | 7980 psi | Weld; ASTM D638 |
Kuraray Genestar™ GR2300 Nylon, 30% Glass Filled Standard V-0 Grade. Delivers increased fluidity and weld strength. Well suited for a wide range of electrical and electronic components. |
|||
Tensile Strength | 55.0 MPa | 7980 psi | 5 mm/min; ISO 527-1 |
Sax Polymers SAXALEN PPC345G30 Polypropylene Copolymer, 30% Glass Filled SAXALEN PPC345G30 is a 30% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers |