Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 27.6 - 34.5 MPa | 4000 - 5000 psi | ASTM D638 |
Mar-Bal MB2000-5 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Tensile Strength | 27.6 - 34.5 MPa | 4000 - 5000 psi | ASTM D638 |
Mar-Bal MB2000-8 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |