Mechanical Properties Metric English Comments
Tensile Strength 30.0 - 50.0 MPa
4350 - 7250 psi
ISO 527
Raschig Group EN 5004 Epoxy Molding Compound
Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo..
Tensile Strength 30.0 - 50.0 MPa
4350 - 7250 psi
ISO 527
Raschig Group EN 5007 Epoxy Molding Compound
Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo..
Tensile Strength 40.0 - 50.0 MPa
5800 - 7250 psi
Compression; ISO 527
Raschig Group MELOPAS® 156 MF Melamine
Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200..
Tensile Strength 40.0 - 50.0 MPa
5800 - 7250 psi
Injection; ISO 527
Raschig Group RALUPOL® 2100 UP Polyester
Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta..
Tensile Strength 38.0 - 50.0 MPa
5510 - 7250 psi
DIN 53455
Isoflon PVDF Polyvinyl Dichloride Fluoropolymer
Fluoropolymer material specifications.Information provided by Isoflon.
Tensile Strength 45.0 - 50.0 MPa
6530 - 7250 psi
ASTM D638
3D Systems Accura® Xtreme White 200 Plastic
Ultra tough white plastic to replace CNC Machined polypropylene and ABS articles FeaturesExceptionally tough and durableUsed for challenging functional assembliesUsed for snap fit assembl..
Tensile Strength 40.0 - 50.0 MPa
5800 - 7250 psi
ISO 527
Bulk Molding Compounds tetra-DUR F 4308 Bulk Molding Compound
UL-licensedTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), thermal stabilit..
Tensile Strength 30.0 - 50.0 MPa
4350 - 7250 psi
ISO 527
Bulk Molding Compounds tetra-DUR F 4401 Bulk Molding Compound
UL-licensed, general purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prot..
Tensile Strength 30.0 - 50.0 MPa
4350 - 7250 psi
ISO 527
Bulk Molding Compounds tetra-DUR L 4305 Bulk Molding Compound
UL-licensed. Anchor wave-isolation.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prote..
Tensile Strength 40.0 - 50.0 MPa
5800 - 7250 psi
ISO 527
Bulk Molding Compounds tetra-DUR F 4306 Bulk Molding Compound
Mechanical high grade standard productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion pr..