Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 5.17 MPa @Strain 100 % |
750 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible MG23B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 5.17 MPa @Strain 100 % |
750 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 2155 Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2155 is a 55 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2155 can be used for extrusion and injection molding healthcare applications.NOTE: All ing.. |
|||
Tensile Strength | 5.17 MPa @Strain 100 % |
750 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 2155G Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2155G is a 55 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2155G can be used for extrusion and injection molding healthcare applicatio.. |
|||
Tensile Strength | 5.17 MPa | 750 psi | Side 2; ASTM D412 |
Arlon 18646B026 0.026" (0.66 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: 11523 Style FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneThis data represents typical values for the production materi.. |
|||
Tensile Strength | 5.17 MPa | 750 psi | Silicone Property; ASTM D412 |
Arlon CP-PC-2951 Silicone Compound This data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division. |
|||
Tensile Strength | 5.17 MPa | 750 psi | Silicone Property; ASTM D412 |
Arlon P29514R015 0.0165" (0.419 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassProduct Advatages:Flexibility: Silicone rubber resists damage due to vibration, frame movement under loa.. |
|||
Tensile Strength | 5.17 MPa | 750 psi | Silicone Property; ASTM D412 |
Arlon P29514R020 0.0205" (0.521 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassAppearance: Red silicone rubber on fiberglass fabric.This data represents typical values for the product.. |
|||
Tensile Strength | 5.17 MPa | 750 psi | Silicone Property; ASTM D412 |
Arlon P29514R020P 0.0205" (0.521 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassThis data represents typical values for the production material. The data should.. |
|||
Tensile Strength | 5.17 MPa | 750 psi | Silicone Property |
Arlon R30370A008 0.008" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 0.001" FEP FilmSide 1: Unsupported/Uncured Silicone RubberSubstrate: 0.003" PTFE coated FiberglassThis data represents typical values for the production material a.. |
|||
Tensile Strength | 5.17 MPa | 750 psi | Silicone Property; ASTM D412 |
Arlon R38026B017 0.017" (0.432 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassSide 2: Uncured Silicone Rubber Interleave: LDPEThis data represents typical values for the production material. The.. |
|||
Tensile Strength | 5.17 MPa | 750 psi | Silicone Property; ASTM D412 |
Arlon Thermabond® 48781A008 0.008" (0.203 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Generation II Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner 1: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style.. |
|||
Tensile Strength | 5.17 MPa | 750 psi | Silicone Property; ASTM D412 |
Arlon Thermabond® R36200A008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated Fiberglass Appearance: Blue silicone gumThis data represents typical values for the production material. The d.. |
|||
Tensile Strength | 5.17 MPa | 750 psi | Silicone Property; ASTM D412 |
Arlon Thermabond® R36211A008 0.008" (0.203 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Generation II Thermabond® NP electrically insulating electronic adhesive. Bonds without primerDesign/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: St.. |
|||
Tensile Strength | 5.17 MPa | 750 psi | Silicone Property |
Arlon R30370A015 0.015" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 0.001" FEP FilmSide 1: Unsupported/Uncured Silicone RubberSubstrate: 0.003" PTFE coated FiberglassThis data represents typical values for the production material a.. |
|||
Tensile Strength | >= 5.17 MPa | >= 750 psi | Compound Property |
Arlon R33991R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |