Polymer Property : Tensile Strength = 48.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 48.0 MPa

@Thickness 0.0440 mm
6960 psi

@Thickness 0.00173 in
ASTM D882-02
NeXolve White Optionox® Polyimide Film
Highly UV durable with excellent weatherability and stability to ozone.Optinox® films and coatings are highly UV durable and exhibit excellent weathering durability, including very high stability ..
Tensile Strength 48.0 MPa
6960 psi
ISO 527-1
Sax Polymers SAXLAC 120U Acrylonitrile Butadiene Styrene
Saxalac 120U is an UV protected easy flowing ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical property data tested..
Tensile Strength >= 48.0 MPa
>= 6960 psi
ISO 37
Austin Novel Materials Texalan® 264D Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Tensile Strength >= 48.0 MPa
>= 6960 psi
ISO 37
Austin Novel Materials Texalan® 764D PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Tensile Strength >= 48.0 MPa
>= 6960 psi
ISO 37
Austin Novel Materials Texalan® 598A Polyether-based TPU
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Tensile Strength 48.0 MPa
6960 psi
5 mm/min; ISO 527-2
CENTROPLAST CENTRODAL MD Polyoxymethylene, Magnetically Detectable
During the modification with POM MD, metal fillings are added to the basic polyoxymethylene, which allows the plastic to be detectable. The excellent machinability, tenacity and dimensional stabilit..