Polymer Property : Tensile Strength = 47.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 47.6 MPa
6900 psi
ASTM D638
Techmer ES Luriblend® POM CO E TL20
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated, Good Wear Resistance and CopolymerProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Tensile Strength 47.6 MPa
6900 psi
ASTM D638
Techmer ES Luriblend® TPX-PA6-95002
Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Tensile Strength 47.6 MPa
6900 psi
ASTM D638
Americas Styrenics STYRON® 675 High Heat Crystal Polystyrene
Product CharacteristicsHigh heatMedium flowFood Contact CompliantUL Classification 94HBTypical ApplicationsThin-walled partsInformation provided by AmericasStyrenics LLC.
Tensile Strength 47.6 - 61.4 MPa
6900 - 8900 psi
Bulk Molding Compounds BMC T14 General Purpose Molding Compound
BMC T14 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T14 is well suited for injection, transfer or compression molding of intricate parts. Typica..
Tensile Strength 47.6 - 61.4 MPa
6900 - 8900 psi
Bulk Molding Compounds BMC A50-MS General Purpose Molding Compound
BMC A50-MS is a medium strength, high appearance, general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A50-MS is well suited for injection, transfer or compres..