Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 45.0 MPa | 6530 psi | ISO 527 |
Premix Thermoplastics PRETECH Halogen-free Engineering Thermoplastics Halogen-free PRETECH engineering thermoplastics enable environmentally friendly and cost efficient V-0 product solutions with excellent mechanical and electrical properties. PRETECH combines high th.. |
|||
Tensile Strength | 45.0 - 60.0 MPa | 6530 - 8700 psi | Injection; ISO 527 |
Raschig Group MELOPAS® 156 MF Melamine Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200.. |
|||
Tensile Strength | 45.0 MPa | 6530 psi | Weld; ASTM D638 |
Kuraray Genestarâ„¢ G1300H Nylon, 30% Glass Filled Standard HB grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm. It is suitable for use in .. |
|||
Tensile Strength | 45.0 MPa | 6530 psi | Weld; ASTM D638 |
Kuraray Genestarâ„¢ G1350H Nylon, 35% Glass Filled Standard HB grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm. It is suitable for use in .. |
|||
Tensile Strength | 45.0 MPa | 6530 psi | ASTM D638 |
KYDEX® 110 Metallic Thermoplastic Fire-rated Sheet Features:For deep or hard to form parts where good finished detail is requiredMore rigid than most thermoplastics, parts deform less when loadedMeets highest standard for chemical resistance for the.. |
|||
Tensile Strength | 45.0 MPa | 6530 psi | ASTM D638 |
KYDEX® 6503 Integral Pearlescent Low Heat Release Aviation Thermoforming Sheet Features:Thicknesses from 0.71 mm to 3.18 mmChemical resistant - easy to clean with aggressive cleanersForms deep draws with low forces when heated to the upper end of forming temperature rangeCrisp.. |
|||
Tensile Strength | 45.0 MPa | 6530 psi | ISO 527 |
Lucite International Diakon® TD542 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Tensile Strength | 45.0 MPa | 6530 psi | DIN 53455 |
Isoflon PVDF Polyvinylidene fluoride Electrical and thermal insulating products with food slipping propertiesChemically inertInformation provided by Isoflon. |
|||
Tensile Strength | 45.0 MPa | 6530 psi | GB/T 1040.2-2006 |
Sichuan Deyang Haton® hFR31 PPS / AR Polyphenylene Sulfide Injection molding, conductiveInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Tensile Strength | 45.0 MPa | 6530 psi | ISO 527-1 |
Sax Polymers SAXATEC 4307 Acrylonitrile Styrene Acrylate SAXATEC 4307 is a high impact resistant, high viscosity and weatherable ASA injection molding grade, characterized by high mechanical strength and good processabilityInformation provided by SAX Poly.. |
|||
Tensile Strength | 45.0 MPa | 6530 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-7195 Polycaprolactone Based TPU Higher mechanical strength, good hydrolytic stability & chemical resistance, weather resistance, heat & fungus resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 45.0 MPa | 6530 psi | DIN EN ISO 527 |
Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy Main Characteristics: Hard; Stiff; Tough; High dimensional stability; High fatigue strength; High weather resistance; Good fire behavior; Suitable for vacuum; Good machinability; Contains PTFE; Stre.. |
|||
Tensile Strength | 45.0 MPa | 6530 psi | ASTM D412 |
Lubrizol Estane® 58070 Thermoplastic Polyurethane Features: Outstanding resiliency, fuel resistance and low temperature flexibility.Uses: Hose and Tube, Injection Molding, Fabric Coating and Wire/CableAvailable in Americas, Europe, Middle East, Afr.. |
|||
Tensile Strength | 45.0 MPa @Temperature 136 °C, Time 605000 sec |
6530 psi @Temperature 277 °F, Time 168 hour |
Air Oven; ASTM D412 |
Lubrizol Estane® 58070 Thermoplastic Polyurethane Features: Outstanding resiliency, fuel resistance and low temperature flexibility.Uses: Hose and Tube, Injection Molding, Fabric Coating and Wire/CableAvailable in Americas, Europe, Middle East, Afr.. |
|||
Tensile Strength | 45.0 MPa | 6530 psi | |
Corbion Purac Blend A High Heat Homopolymer PLA Heat resistance higher than typical PLA is achieved by addition of a nucleating agent and PDLA homopolymer. Data is for samples produced from Puralact L and D lactide monomers; Purac also produces .. |
|||
Tensile Strength | 45.0 - 50.0 MPa | 6530 - 7250 psi | ASTM D638 |
3D Systems Accura® Xtreme White 200 Plastic Ultra tough white plastic to replace CNC Machined polypropylene and ABS articles FeaturesExceptionally tough and durableUsed for challenging functional assembliesUsed for snap fit assembl.. |
|||
Tensile Strength | 45.0 MPa | 6530 psi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 MX6 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grade, reinforced with 10% hybrid mineral-glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good su.. |
|||
Tensile Strength | 45.0 MPa | 6530 psi | ISO 37 |
BASF Elastollan 1185 A M TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tensile Strength | 45.0 MPa | 6530 psi | ISO 37 |
BASF Elastollan 564 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and a high abrasion resistance.Typical Applications: Heel top-pieces, castor tyres and parts requiri.. |
|||
Tensile Strength | 45.0 MPa @Strain 2.00 %, Temperature 23.0 °C |
6530 psi @Strain 2.00 %, Temperature 73.4 °F |
50 mm/min; ISO 527-2 |
BASF Elastollan R 3000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Tensile Strength | 45.0 MPa | 6530 psi | ISO 37 |
BASF Elastollan S 64 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | >= 45.0 MPa | >= 6530 psi | ISO 37 |
Austin Novel Materials Texalan® 295A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tensile Strength | >= 45.0 MPa | >= 6530 psi | ISO 37 |
Austin Novel Materials Texalan® 498A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Strength | 45.0 MPa | 6530 psi | ISO 37 |
BASF Elastollan 2180 A TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tensile Strength | 45.0 MPa | 6530 psi | ISO 37 |
BASF Elastollan 560 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and a high abrasion resistance.Typical Applications: Heel top-pieces, castor tyres and parts requiri.. |
|||
Tensile Strength | 45.0 MPa | 6530 psi | ISO 37 |
BASF Elastollan S 98 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | >= 45.0 MPa | >= 6530 psi | ISO 37 |
Austin Novel Materials Texalan® 698A Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Strength | >= 45.0 MPa | >= 6530 psi | ISO 37 |
Austin Novel Materials Texalan® 798A PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Tensile Strength | 45.0 MPa | 6530 psi | ISO 37 |
BASF Elastollan S 60 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 45.0 MPa | 6530 psi | ISO 527 |
Lucite International Diakon® ST45G8 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed by in.. |