Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 29.0 MPa | 4210 psi | ASTM D638 |
Kolon KOCETAL® EL306 Toughened Grade Acetal Resin Flexible grade. Applications: Flexible products. Information provided by API-Kolon. |
|||
Tensile Strength | 29.0 MPa | 4210 psi | ASTM D638 |
Kolon KOPEL® KP3855FB Polyester Elastomer Resin (TPE) High flow, Air bag cover |
|||
Tensile Strength | 29.0 MPa | 4210 psi | ASTM D412 |
GRECO ISOTHANE 1090AE Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are Poly(adipate)ester based thermoplastic polyurethanes with good balanced qualities. They exhibit good toughness, abrasive resistance, solvent resistance, and transp.. |
|||
Tensile Strength | 29.0 MPa | 4210 psi | ISO 527 |
Lucite International Elvakon® 4490 High Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Tensile Strength | 29.0 MPa | 4210 psi | ISO 527 |
Lucite International Elvakon® 4494 Low Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Tensile Strength | 29.0 MPa | 4210 psi | TD; ISO 527 |
Lucobit Lucofin® 1400HN Powder Ethylene Butyl Acrylate Lucofin 1400HN Powder is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN Powder is softer and more flexible than ethy.. |
|||
Tensile Strength | >= 29.0 MPa | >= 4210 psi | Grade A |
Shandong Dongyue Polymer DF-11 PTFE Molding Powder (Micronized Particles) Usage: The resin is mainly used as an insulating film for electric applications, the products of thin wall, seal, gasket, club, panel, tube, axletree, seal ring, and loop.Packing: PTFE is packed in .. |
|||
Tensile Strength | >= 29.0 MPa | >= 4210 psi | Grade A |
Shandong Dongyue Polymer DF-16 PTFE Molding Powder (Micronized Particles) Usage: The resin can be used as the general required electric source, which is suitable for making film, the products of thin wall, seal, gasket, club, panel, tube, axletree, seal ring, loop, fillin.. |
|||
Tensile Strength | >= 29.0 MPa | >= 4210 psi | Grade A |
Shandong Dongyue Polymer DF-17 PTFE Molding Powder (Micronized Particles) Usage: The resin is mainly used as the packing products resource and packing pelletized resource, which can be processed to film, the products of thin wall, seal, gasket, club, panel, tube, axletree.. |
|||
Tensile Strength | 29.0 MPa | 4210 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-2190 Polycaprolactone Based TPU Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 29.0 MPa | 4210 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8254 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 29.0 MPa | 4210 psi | ASTM D412 |
Lubrizol ESTANE® 58091 Ester Based Thermoplastic Polyurethane Features: High stiffness TPU alloyUses: Flat Die/Cast Sheet Extrusion, Profile Extrusion and Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided b.. |