Polymer Property : Tensile Strength = 421 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 2.90 MPa
421 psi
Shin-Etsu Silicones KE-40RTV Silicone, RTV
Information Provided by Shin-Etsu Silicones of America, Inc.
Tensile Strength 2.90 MPa

@Strain 100 %
421 psi

@Strain 100 %
ISO 37
BASF Elastollan S 70 AWH TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
Tensile Strength 2.90 - 7.00 MPa
421 - 1020 psi
ASTM D 638
API Megol AM DP1741 SEBS Adhesion Modified Overmolding for PA
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as ..
Tensile Strength 2.90 MPa
421 psi
average; perpendicular to plane; ASTM C297
3A Composites Core Materials AIREX® T92.110 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,..
Tensile Strength 2.90 MPa
421 psi
ISO 37
AlphaGary Evoprene™ GC 5696 SEBS Thermoplastic Elastomer
Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can..