Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 2.52 MPa | 366 psi | ASTM D412 |
Northstar Polymers MPP-A60A Liquid Castable Polyurethane MPP-A60A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |