Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 20.0 - 25.0 MPa | 2900 - 3630 psi | DIN 53455 |
Isoflon FEP Fluorinated Ethylene Propylene Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Tensile Strength | 20.0 - 25.0 MPa | 2900 - 3630 psi | ASTM D4894 |
Isoflon PTFE + 40% Bronze Polytetrafluoroethylene with 40% Bronze Properties:Excellent wear and compression resistance (low cold creep)Good thermal conductivityImproved coefficient of friction when combined with Mos² or graphiteApplications: Dynamic seals for .. |
|||
Tensile Strength | 13.5 - 25.0 MPa | 1960 - 3630 psi | Moulding Direction; BS2782:Pt3 |
Dalau Dalcon 018 85% Virgin PTFE, 15% Graphite Applications & Industries: General: Graphite filler improves the sliding properties & thermal conductivity of PTFE and has one of the lowest coefficient of frictions. It has low wear in water and is.. |
|||
Tensile Strength | 12.0 - 25.0 MPa | 1740 - 3630 psi | Moulding Direction; BS2782:Pt3 |
Dalau Dalcon 021 75% Virgin PTFE, 25% Carbon Coke Applications & Industries: General: Carbon / Coke (soft) filler is good in dry running conditions, adds to the creep resistance, increases the hardness and raises the thermal conductivity of PTFE; C.. |
|||
Tensile Strength | 13.5 - 25.0 MPa | 1960 - 3630 psi | Moulding Direction; BS2782:Pt3 |
Dalau Dalcon 018 85% Virgin PTFE, 15% Graphite Applications & Industries: General: Graphite filler improves the sliding properties & thermal conductivity of PTFE and has one of the lowest coefficient of frictions. It has low wear in water and is.. |
|||
Tensile Strength | 12.0 - 25.0 MPa | 1740 - 3630 psi | Moulding Direction; BS2782:Pt3 |
Dalau Dalcon 021 75% Virgin PTFE, 25% Carbon Coke Applications & Industries: General: Carbon / Coke (soft) filler is good in dry running conditions, adds to the creep resistance, increases the hardness and raises the thermal conductivity of PTFE; C.. |