Polymer Property : Tensile Strength = 3500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 24.1 MPa
3500 psi
ASTM D412
S&E Specialty Polymers TufTech™ GA-1030 PVC Compound
Application: A 60°C, TW, THW PVC based insulation compound.Information provided by S&E Specialty Polymers
Tensile Strength 24.1 MPa
3500 psi
ASTM F152
Garlock GRAPH-LOCK® 3125TC Graphite Sheet Gasketing, Steel Insert
A laminated graphite sheet with a 316SS tang insert.Pure exfoliated graphite flake material excels in extreme conditions, withstanding heat, pressure, and aggressive chemicalsProven fire-safeSeals e..
Tensile Strength 24.1 MPa
3500 psi
Lucite International Elvacite ® 2014 Acrylic Resin
Elvacite® 2014 is a medium molecular weight methyl methacrylate copolymer. 2014 is the softest and most flexible of the Elvacite® copolymer grades. It provides good pigment wetting. ElvaciteÂ..
Tensile Strength 24.1 MPa
3500 psi
Solvay Chemicals NOCOLOK® Braze Paste x43-7
A braze paste specifically formulated for providing viscous mixture of flux and alloy for brazing noncladded aluminum materials, including 1100, 3001 and 6061 series aluminum. Uses: Automotive Sect..
Tensile Strength 24.1 MPa
3500 psi
Solvay Chemicals NOCOLOK® Braze Paste x47-12
A braze paste specifically formulated for providing viscous mixture of flux and alloy for brazing noncladded aluminum materials. Paste can be dispensed manually by brush, syringe, or with automatic ..
Tensile Strength 24.1 MPa
3500 psi
ASTM D638
Techmer ES HiFill® ABS 0350
Availability: North AmericaFeatures: High DensityForms: PelletsProcessing Method: Extrusion MoldingInformation provided by TP Composites, Inc.
Tensile Strength 24.1 MPa
3500 psi
Solvay Chemicals NOCOLOK® Braze Paste x45-10
NOCOLOK® Braze Paste X45-10 is specifically formulated for providing viscous mixture or flux and alloy for brazing noncladded aluminum materials. Uses: Automotive Sector, Commercial & Residentia..
Tensile Strength 24.1 MPa
3500 psi
ASTM D638, ASTM D1708
ScanTube FEP Tubing
Information provided by ScanTube, Inc.
Tensile Strength 24.1 MPa
3500 psi
ASTM D638, ASTM D1708
ScanTube MFA Tubing
Information provided by ScanTube, Inc.
Tensile Strength 24.1 MPa
3500 psi
ASTM D638, ASTM D1708
ScanTube PTFE Tubing
Information provided by ScanTube, Inc.
Tensile Strength >= 24.1 MPa
>= 3500 psi
Master Bond EP21TDCHT-LO Room Temperature Curing, Toughened Two Component Epoxy
Master Bond Polymer Adhesive EP21TDCHT-LO is a two component epoxy adhesive formulated to cure at room temperature or more rapidly at elevated temperatures, with a very forgiving and convenient one ..
Tensile Strength >= 24.1 MPa
>= 3500 psi
Master Bond LED401 One Component LED Curable Adhesive System
Master Bond LED401 is a highly innovative, one part LED type system that cures fully upon exposure to a 405 nm wavelength light source where the presence of any UV light is minimal or incidental. In..
Tensile Strength >= 24.1 MPa
>= 3500 psi
Master Bond LED403Med USP Class VI, One Component, LED Curable System
Master Bond LED403Med is a one part LED system that cures fully upon exposure to a 405 nm wavelength light that is generated by an LED source and. In fact, this material will fully cure tack-free wi..
Tensile Strength 24.1 MPa
3500 psi
AlphaGary GW 3010 LCF P Flame Retardant Polyvinyl Chloride
60°C or 75°C rated jacket compound.
Tensile Strength 24.1 MPa
3500 psi
Henkel Hysol EA 9323 Paste Adhesive System
Viscous, but pourable, liquid adhesive that yields tough, durable adhesive bonds over a wide temperature range.Application: Structural Repair