Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 21.37 MPa | 3099 psi | Typical properties of film cast form toluene solution; ASTM D412 |
Kraton® D1161 K (SIS) Linear Triblock Copolymer Description: Kraton D1161 K is a clear, linear triblock copolymer based on styrene and isoprene, with a polystyrene content of 15%. It is supplied from North America in the physical form identified:.. |
|||
Tensile Strength | 21.37 MPa | 3099 psi | Measured on films cast from a toluene solution; ASTM D412 |
Kraton® D1161 P (SIS) Linear Triblock Copolymer Description: Kraton D1161 P is a clear, linear triblock copolymer based on styrene and isoprene, with a polystyrene content of 15%. It is supplied from North America in the physical form identified:.. |