Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 3.50 MPa | 508 psi | |
Shin-Etsu Silicones KE-1204 B Silicone, Potting/Encapsulation RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tensile Strength | 3.50 MPa | 508 psi | ASTM D412 |
Dynasol Solprene® 4321 Thermoplastic Rubber (SBS) Solprene 4321 is a linear block copolymer of styrene and butadiene, with 32% styrene content, most of it forming polystyrene block, which gives the polymer a thermoplastic behavior. It has a non-st.. |
|||
Tensile Strength | 3.50 MPa @Strain 20.0 % |
508 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan 1185 A M TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tensile Strength | 3.50 MPa @Strain 100 % |
508 psi @Strain 100 % |
ISO 37 |
BASF Elastollan C 75 A HPM TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tensile Strength | 3.50 MPa | 508 psi | ISO 37 |
AlphaGary Evoprene™ Super G 946 SEBS Thermoplastic Elastomer Evoprene™ Super G compounds are high performance styrene ethylene- butylene styrene based thermoplastic elastomers. Evoprene™ Super G has improved heat resistance and improved recovery properties.. |
|||
Tensile Strength | 3.50 - 7.00 MPa | 508 - 1020 psi | ASTM D 638 |
API Megol AM SV/PS SEBS Adhesion Modified Overmolding for PS Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
Tensile Strength | 3.50 MPa @Strain 20.0 % |
508 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan 1185 A FHF TPUR Flame Retardant Halogen Free Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tensile Strength | 3.50 MPa @Strain 20.0 % |
508 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan C 85 A HPM TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tensile Strength | 3.50 MPa | 508 psi | ISO 37 |
AlphaGary Evoprene™ 068 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Tensile Strength | 3.50 MPa | 508 psi | ISO 37 |
AlphaGary Evoprene™ 084 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |