Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 202 MPa | 29300 psi | 5 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 126F9 Nylon 6, 45% Glass Fiber SAXAMID 126F9 is a polyamide 6 injection-molding-grade reinforced with 45% glass fibers.Information provided by SAX Polymers |