Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 19.77 MPa | 2867 psi | Product Property; Arlon SQA-TMS-048 |
Arlon T3030-R004 0.030" (0.762 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate Design/Construction: Side 1: Cured Fusible Silicone RubberSubstrate: 25% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester FilmArlon MOX-Tape® Fiberglass Reinforced T.. |