Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1.90 MPa @Strain 100 % |
276 psi @Strain 100 % |
ISO 527 |
Premix Thermoplastics PRE-ELEC® TPE 1502 Conductive Thermoplastic Compound PRE-ELEC® TPE 1502 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
Tensile Strength | 1.90 MPa @Strain 100 % |
276 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible G92D Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 1.90 - 16.9 MPa | 276 - 2450 psi | EVA/NBR Strippable Compounds |
TIMCAL ENSACO™ 210G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |
|||
Tensile Strength | 1.90 - 16.9 MPa | 276 - 2450 psi | EVA/NBR Strippable Compounds |
TIMCAL ENSACO™ 250G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |
|||
Tensile Strength | >= 1.90 MPa | >= 276 psi | in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® R82.110 High Performance Structural Foam AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines outstanding fire resistance with low smoke and toxicity, along with excellent dielectric properties. It has a good strength to .. |
|||
Tensile Strength | 1.90 MPa | 276 psi | average; perpendicular to plane; ASTM C297 |
3A Composites Core Materials AIREX® T92.80 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r.. |