Polymer Property : Tensile Strength = 250 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 250 MPa

@Thickness >=1.50 mm
36300 psi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 527; IEC/EN 60893-2 5.6
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet
High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr..
Tensile Strength 250 MPa

@Thickness >=1.50 mm
36300 psi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 527; IEC/EN 60893-2 5.6
Elektro-Isola G-Etronax M Melamine, Glass Fabric Reinforcement, White, Sheets
Description: Melamine-based composite material reinforced with glass fabric. High arc resistance and tracking resistance. Flame-resistant. Self-extinguishing.Information provided by Elektro-Isola
Tensile Strength >= 250 MPa
>= 36300 psi
IEC 1212-2 5.7
Hippe EP GM 202 Glass Mat Reinforced Epoxy Resin - Sheet
Tensile Strength >= 250 MPa
>= 36300 psi
IEC 1212-2 5.7
Hippe PI GC 301 Woven Glass Cloth Reinforced Phenolic Sheet
Used in electrical and mechanical applications. Very good mechanical and electrical properties at high temperature.Information provided by Hippe.
Tensile Strength >= 250 MPa
>= 36300 psi
IEC 1212-2 5.7
Hippe EP GM 201 Glass Mat Reinforced Epoxy Resin - Sheet
Used in mechanical and electrical applications. Extremely high mechanical strength at moderate temperature. Very good electrical properties under high humidity.Information provided by Hippe.
Tensile Strength >= 250 MPa
>= 36300 psi
IEC 1212-2 5.7
Hippe EP GM 203 Glass Mat Reinforced Epoxy Resin - Sheet
Tensile Strength >= 250 MPa
>= 36300 psi
IEC 1212-2 5.7
Hippe EP GM 204 Glass Mat Reinforced Epoxy Resin - Sheet
Tensile Strength 250 MPa
36300 psi
y; IPC TM-650 2.4.18.3
Arlon 35N Fast Cure Polyimide Laminate and Prepreg
High reliability and high temperature material35N is a pure polyimide laminate and prepreg system for applications requiring high temperature performance. High Tg results in low Z-direction expansi..