Polymer Property : Tensile Strength = 2320 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 12.0 - 16.0 MPa
1740 - 2320 psi
molded; ASTM D4745
Guarniflon PTFE G456 Polytetrafluoroethylene 25% Hard Carbon
PTFE G Special Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high w..