Tensile Strength 225 MPa
32600 psi
5 mm/min; ISO 527-1
Sax Polymers SAXAMID 226F8 Nylon 6.6, 40% Glass Fiber
SAXAMID 226F8 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 40% glass fibers. It has very high mechanical strength.Information provided by SAX Polymers