Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 136 MPa | 19700 psi | Y direction; RT; ASTM D638 |
Rogers Corporation RO4835 Hydrocarbon Ceramic Laminate, Improved Oxidation Resistance Features and Benefits:Significantly improved oxidation resistance compared to typical thermoset microwave materialsDesigned for performance sensitive, high volume applicationsLow loss - Excellent el.. |
|||
Tensile Strength | 136 MPa | 19700 psi | 12µm polyimide/9µm copper; ASTM D882-02 |
NeXolve TR-Clad™ Flexible Polyimide Laminate The lightest weight copper clad laminates available.TR-Clad™ Flexible Laminates are both the lowest weight and lowest dielectric constant of copper/polyimide laminates available. Additionally, TR.. |
|||
Tensile Strength | 136 MPa | 19700 psi | 5.0 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea.. |
|||
Tensile Strength | 136 MPa | 19700 psi | 5 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK) AV-722 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding.. |
|||
Tensile Strength | 136 MPa | 19700 psi | GB/T 1040.2-2006 |
Sichuan Deyang Haton® hGR31M1 Polyphenylene Sulfide Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |