Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 11.8 MPa | 1710 psi | ASTM D412 |
S&E Specialty Polymers GTPE-2203G1 PVC Application: RoHS compliant, 105° C, flexible, oil resistant TPE jacketing material with extremely good low temperature properties.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 11.8 MPa | 1710 psi | ASTM D412 |
S&E Specialty Polymers TufFlex™ GA-509-75 TPE Compound Application: A UL listed, sunlight resistant, 75°C rated, UL1277 power limited and control cable jacketing compound for CMX, CL2 and CL3 applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 11.8 MPa @Temperature 100 °C, Time 864000 sec |
1710 psi @Temperature 212 °F, Time 240 hour |
Aged |
S&E Specialty Polymers TufFlex™ GA-509-75 TPE Compound Application: A UL listed, sunlight resistant, 75°C rated, UL1277 power limited and control cable jacketing compound for CMX, CL2 and CL3 applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | >= 11.8 MPa | >= 1710 psi | ASTM D 638 |
Karina E CAK 85-48/1 Black PVC Compound Reclaimed PVC compound recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 11.8 MPa | >= 1710 psi | ASTM D 638 |
Karina TR-700-35/1 Ivory PVC Compound PVC compound with addition of nitrile rubber, recommended for injection of solesInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 11.8 MPa | >= 1710 psi | ASTM D 638 |
Karina 752D02/101-AT-IS Yellow PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 11.8 MPa | >= 1710 psi | ASTM D 638 |
Karina 833D10/184-AY-IS-AS White PVC Compound PVC compound with additive anti-UV, flame retardant, and fungicide; recommended for extrusion and roll pressed laminated.Information provided by Karina Indústria e Comércio de Plásticos Ltd.. |
|||
Tensile Strength | >= 11.8 MPa | >= 1710 psi | ASTM D 638 |
Karina E 754-10/426-AT-IS White PVC Compound White non-toxic PVC compound, recommended for general extrusion.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | 11.8 MPa | 1710 psi | |
Shin-Etsu Silicones LIMSâ„¢ KEG2001-50A/B Elastomer KEG2001-50 is a very fast cure type liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enou.. |
|||
Tensile Strength | 11.8 MPa | 1710 psi | 500 in/min; ASTM D638 |
Teknor Apex Sinvicomp SHE 5600 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Ethylene Oxide Sterilizable Uses: Medical/Healthcare Applications Forms: GranulesInformation Provided by Teknor Apex |
|||
Tensile Strength | 11.8 MPa | 1710 psi | ASTM D412 |
Dynasol Solprene® 9340 Multi-branched Thermoplastic Rubber (Multi-branched SBS) Solprene® 9340 is a 66/34 Butadiene-Styrene multi arm copolymer, polymerized in solution process. It has a non-staining FDA approved antioxidant system for food contact applications and it is essen.. |
|||
Tensile Strength | >= 11.8 MPa | >= 1710 psi | After 168 H in Air Oven at 100°C; NBR NM-IEC 60811-1-2 |
Karina 802D35/1-E-AC-LF Ivory PVC Compound Heavy metal free and flame retardant PVC compound, recommended for coaxial cables jackets.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |