Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 12.0 - 16.0 MPa | 1740 - 2320 psi | molded; ASTM D4745 |
Guarniflon PTFE G456 Polytetrafluoroethylene 25% Hard Carbon PTFE G Special Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high w.. |