Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 10.3 MPa | 1500 psi | ASTM D638 |
Quadrant EPP Fluorosint® 207 PTFE, Compression Molded Synthetic Mica-filled PTFE (ASTM Product Data Sheet) |
|||
Tensile Strength | 10.3 MPa | 1500 psi | |
Parker Chomerics CHO-SHRINK® Tubing Conductive Heat Shrinkable EMI Shielding Description: CHO-SHRINK tubing is a heat shrinkable polyolefin manufactured to MIL-R-46846 Type 5, modified to provide effective 360° EMI shielding for cables. CHO-SHRINK tubing offers significant .. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | across grain; ASTM F152 |
Garlock 2900 Compressed Aramid Fiber Gasketing, Nitrile Binder Aramid fibers with a nitrile binder.Ideal for utility servicesExcellent sealabilityImproved thermal stabilityGood for general serviceMedia: Water, aliphatic hydrocarbons, oils, gasolineInformation .. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | across grain; ASTM F152 |
Garlock 2940 Compressed Aramid Fiber Gasketing, SBR Binder Aramid fibers with a Styrene-Butadiene (SBR) Binder.Ideal for utility servicesExcellent sealabilityImproved thermal stabilityGood for general serviceMedia: Water, aliphatic hydrocarbons, oils, gasol.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | across grain; ASTM F152 |
Garlock 2950 Compressed Aramid Fiber Gasketing, Nitrile Binder Aramid fibers with a nitrile binder.Ideal for utility servicesExcellent sealabilityImproved thermal stabilityGood for general serviceMedia: Water, aliphatic hydrocarbons, oils, gasolineInformation .. |
|||
Tensile Strength | >= 10.3 MPa | >= 1500 psi | |
Garlock 509 Butyl Sheet Rubber Style #509 is a branded, chloro-butyl sheet rubber product.Information provided by Garlock Rubber Technologies |
|||
Tensile Strength | >= 10.3 MPa | >= 1500 psi | |
Garlock 5260 Neoprene Sheet Rubber This blended neoprene sheet is used where good oil, petroleum, ozone and weathering-resistance is needed.Black, smooth finishInformation provided by Garlock Rubber Technologies |
|||
Tensile Strength | >= 10.3 MPa | >= 1500 psi | |
Garlock 5360 Nitrile Sheet Rubber Nitrile sheet is primarily used for applications where resistance to oil, solvents and fuels is required.Style #5360 is a medium-hard, premium-grade nitrile sheet, also available in 40, 50, 70 and 8.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | across grain; ASTM F152 |
Garlock 5500 Compressed Inorganic Fiber Gasketing, Nitrile Binder Inorganic fibers with a nitrile binder.Inorganic fiber gasketing offers excellent thermal stability with minimal weight lossReduced creep relaxation and improved torque retention provide optimal sea.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | across grain; ASTM F152 |
Garlock 5507 Compressed Inorganic Fiber Gasketing, EPDM Binder Inorganic fibers with an EPDM binder.Inorganic fiber gasketing offers excellent thermal stability with minimal weight lossReduced creep relaxation and improved torque retention provide optimal seala.. |
|||
Tensile Strength | >= 10.3 MPa | >= 1500 psi | |
Garlock 563 EPDM Sheet Rubber Excellent general purpose gasket materials for air, hot and cold water, saturated steam and exterior service.Black, smooth finish. Excellent resistance to weathering, ozone and UV exposure. It prov.. |
|||
Tensile Strength | >= 10.3 MPa | >= 1500 psi | |
Garlock 7797 Neoprene Sheet Rubber This blended neoprene sheet is used where good oil, petroleum, ozone and weathering-resistance is needed.Black, smooth cloth finishInformation provided by Garlock Rubber Technologies |
|||
Tensile Strength | 10.3 MPa | 1500 psi | ASTM D412 |
Garlock 7992 Neoprene Rubber Diaphragm, Fabric Insert Neoprene rubber with 22oz. hose duck fabric insertCombines elasticity and extensibility of rubber with strength of fabric insert. Specially compounded in varying burst strengths for almost any serv.. |
|||
Tensile Strength | >= 10.3 MPa | >= 1500 psi | |
Garlock SBR Extruded Skirtboard SBR rubber extruded skirtboard for protection applicationsInformation provided by Garlock Rubber Technologies |
|||
Tensile Strength | 10.34 MPa | 1500 psi | Typical properties of film cast from toluene solution; ASTM D412 |
Kraton® D1163 P (SIS) Linear Triblock Copolymer Description: Kraton D1163 P is a clear, linear triblock copolymer based on styrene and isoprene, with a polystyrene content of 15%. It is supplied from North America in the physical form identified:.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | across grain; ASTM F152 |
Garlock 9800 Compressed Carbon Fiber Gasketing, SBR Binder Carbon fibers with a SBR binder.Carbon fiber gasketing excels in harshest conditions- intense heat, high pressure, saturated steam and hot oilsLaboratory tested for fire safetyMaintains effective se.. |
|||
Tensile Strength | >= 10.3 MPa | >= 1500 psi | ASTM D412 Method A |
Seals Eastern 7040 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | Silicone Property; ASTM D412 |
Arlon HS930-10R##-P4 0.030" (0.762 mm) Self-Fusing Silicone Tape (Rectangular, Unsupported) Description: High Strength, 1 inch wide, 30 mil thick, Red, Rectangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicat.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | Silicone Property; ASTM D412 |
Arlon P3272-10Rxx-P4 0.030" (0.762 mm) Cured Self-Fusing Silicone Tape (Rectangular, Unsupported) Description: High strength self-fusing silicone tapeDesign/Construction: Interleave: PolyethyleneRubber: Cured Self-Fusing Silicone Rubber Cross-Section: 1” wide RectangularAppearance: Red silicone.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | Silicone Property; ASTM D412 |
Arlon T3030-R004 0.030" (0.762 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate Design/Construction: Side 1: Cured Fusible Silicone RubberSubstrate: 25% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester FilmArlon MOX-Tape® Fiberglass Reinforced T.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | |
AlphaGary Garathane™ X 05-309 A3 Polyurethane based compound Abrasion & Slip Resistant |
|||
Tensile Strength | 10.3 MPa | 1500 psi | |
AlphaGary PVC 2215/3X-55 Black 1000 Polyvinyl Chloride Thermoplastic Molding grade for grommets and connectors with fungus resistance |
|||
Tensile Strength | 10.3 MPa | 1500 psi | Adhesion |
Atom Adhesives AA-DUCT 905 Epoxy Adhesive AA-DUCT 905 is a single component epoxy, formulated with pure silver powder combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | |
Teknor Apex Elexar® EL 1934A Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical properti.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | |
AlphaGary PVC 7731 Polyvinyl Chloride Thermoplastic Automotive Molding |
|||
Tensile Strength | 10.3 MPa | 1500 psi | |
AlphaGary PVC GM 5055 Natural Polyvinyl Chloride Thermoplastic A 105°C rated, lead & cadmium free, UL-94 V2 molding compound |
|||
Tensile Strength | 10.3 MPa | 1500 psi | |
AlphaGary PVC GM 5065 Natural Polyvinyl Chloride Thermoplastic A 105°C rated, lead & cadmium free, UL-94 V2 molding compound |
|||
Tensile Strength | 10.3 MPa | 1500 psi | |
AlphaGary PVC GM 5075 Polyvinyl Chloride Thermoplastic A 105°C rated, lead & cadmium free, UL-94 V2 molding compound |
|||
Tensile Strength | 10.3 MPa | 1500 psi | ASTM D638 |
Quadrant EPP Semitron® ESd 500 HR PTFE, static dissipative, compression molded (ASTM Product Data Sheet) |