Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 10.3 MPa | >= 1490 psi | ASTM D412 |
S&E Specialty Polymers G-04-036ESD PVC Application: High Performance, PVC based compound with antistatic properties. G-04-036ESD is suitable for Gamma radiation sterilization.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 10.3 MPa | 1490 psi | ASTM D638 |
S&E Specialty Polymers GM-3950-095 PVC Non-toxic PVC material designed for molding applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 10.3 MPa | 1490 psi | ASTM D638 |
S&E Specialty Polymers GTPO8280 NATURAL PVC Application: EPDM Based flexible polyolefin compound.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 10.3 MPa @Strain 100 % |
1490 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A8504 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 10.3 MPa @Strain 100 % |
1490 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B85UB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 10.3 MPa @Strain 100 % |
1490 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B90T0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 10.3 MPa @Strain 100 % |
1490 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV-3766 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength | 10.3 MPa @Strain 100 % |
1490 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3875 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength | 10.3 MPa | 1490 psi | ASTM D412 |
S&E Specialty Polymers TufTech™ GM-3958-095 PVC Compound Application: A clear, non-toxic, extrusion compound for food contact use.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 10.3 MPa @Strain 100 % |
1490 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B9000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 10.3 MPa @Strain 100 % |
1490 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible G8024 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 10.3 MPa | 1490 psi | ASTM D412 |
Kraton® G1643 M (SEBS) Linear Triblock Copolymer Description: Kraton G1643 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 20%. It is supplied from North America in the physical form ide.. |
|||
Tensile Strength | 10.3 MPa | 1490 psi | Measured on extrusion cast film; ASTM D412 |
Kraton® G1645 M (SEBS) Linear Triblock Copolymer Description: Kraton G1645 M is a linear triblock copolymer based on styrene and ethylene/butylene. It is supplied from North America in the physical form identified: Kraton G1645 MO - supplied as a .. |
|||
Tensile Strength | 10.3 MPa | 1490 psi | |
Momentive Performance Materials TSE 2267 Heat Cured Rubber - High Duro Translucent Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 10.3 MPa | 1490 psi | ASTM D638 |
Saint-Gobain Rulon® LR Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |