Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 993 MPa | 144000 psi | ASTM D638 |
Quantum Composites AMC™ 8595 55% Carbon Fiber Reinforced Vinyl Ester SMC AMC™ 8595 is a vinyl ester engineered structural composite molding compound with continuous, unidirectional carbon fibers. It is designed for compression molding of components requiring high struc.. |
|||
Tensile Strength | 990 MPa | 144000 psi | |
Plansee DENSIMET® D2M Tungsten-Nickel-Molybdenum-Iron Alloy Characteristics:Easy processingHigh densityPrecision forming and machiningHigh ductilityHigh strength100 % impermeableTypical Applications:Balancing weights in motors and drive componentsVibration d.. |