Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 9.65 MPa | 1400 psi | ASTM D638 |
S&E Specialty Polymers GTP09005 PVC A proprietary, low gravity, non-halogen based flame retardant thermoplastic polyolefin designed for extrusion in wire and cable applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 9.65 MPa | 1400 psi | ASTM D638 |
S&E Specialty Polymers GTP09008-1 PVC Non-halogen flame retardant TPO for wire and cable extrusion.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 9.65 MPa | 1400 psi | ASTM D412 |
S&E Specialty Polymers TufTech™ G-3570 PVC Compound Application: A PVC compound designed for work boot and boat shoe soling applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 9.65 MPa @Strain 100 % |
1400 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A8500 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Tensile Strength | 9.65 MPa @Strain 100 % |
1400 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A8501 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Tensile Strength | 9.65 MPa @Strain 100 % |
1400 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B83UB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 9.65 MPa @Strain 100 % |
1400 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible D8500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 9.65 MPa @Strain 100 % |
1400 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible D9000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 9.65 MPa @Strain 100 % |
1400 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R336AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 9.65 MPa | 1400 psi | Typical |
Garlock 4160 Natural Sheet Rubber Excellent general purpose gasket materials for air, hot and cold water, saturated steam and exterior service.Red, smooth finishInformation provided by Garlock Rubber Technologies |
|||
Tensile Strength | 9.65 MPa | 1400 psi | across grain; ASTM F152 |
Garlock 706 Compressed Inorganic Fiber Gasketing, Nitrile Binder Inorganic fibers with a nitrile binder.Inorganic, asbestos-free fibers offer superior performance in saturated and superheated steamThermally stable fibers retain effective seal even during thermal .. |
|||
Tensile Strength | 9.65 MPa | 1400 psi | Machine Direction; Injection molded sample tested at 10 in/min with Die D; ASTM D412 |
Kraton® D2104 DI-N (SBS) Compound Description: Kraton D2104 DI-N is an easy processing, general purpose material designed for a wide variety of applications. It is supplied from North America in the physical form identified: D2104 D.. |
|||
Tensile Strength | 9.65 MPa | 1400 psi | Silicone Property; ASTM D412 |
Arlon R39118R037L 0.037" (0.940 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyester Release Liner Transfer Pressure Sensitive Adhesive: Silicone PSASide 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Cured Silicone Rubber.. |
|||
Tensile Strength | 9.65 MPa | 1400 psi | Silicone Property; ASTM D412 |
Arlon T4020-R002 0.020" Cured, Fusible Silicone Rubber with Fiberglass Substrate 0.5 inch wide, 20 mil thick, red, rectangular cross-section, fusible silicone tape.Design/Construction:Side 1: Cured Fusible Silicone RubberSubstrate: 15% Sinusoidal FiberglassSide 2: Cured Fusibl.. |
|||
Tensile Strength | 9.65 MPa | 1400 psi | |
AlphaGary Garathane™ X 96-322 A Polyurethane based compound Abrasion & Slip Resistant |
|||
Tensile Strength | 9.65 MPa | 1400 psi | |
AlphaGary Garaflex™ O 9939NA Olefinic Thermoplastic Elastomer Garaflex™ O is a flame retarded, olefinic thermoplastic elastomer105°C rated flame retardant olefinic TPE for flat ribbon cable and heat tracing cable |