Tensile Strength 130 MPa
18900 psi
at Break (NYP); ISO 527-1/-2
Quadrant EPP Duratron® PBI CU60 compression moulded (ISO Data)
Duratron CU60 PBI is very “clean” in terms of ionic impurity and does not outgas (except water). These characteristics make this material extremely attractive to high-tech industries such as semic..
Tensile Strength 130 MPa
18900 psi
ASTM D638
Solvay Specialty Polymers Veradel® 3330GF Polyethersulfone (PESU), 30% Glass Fiber
Veradel® 3330GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, ..
Tensile Strength 130 MPa
18900 psi
ASTM D638
Solvay Specialty Polymers Veradel® 3430GF Polyethersulfone (PESU), 30% Glass Fiber
Veradel® 3430GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, ..
Tensile Strength 130 MPa
18900 psi
GB/T 1040.2-2006
Sichuan Deyang Haton® hGR20 Polyphenylene Sulfide, Glass Fiber Reinforced
Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD
Tensile Strength 130 MPa
18900 psi
5 mm/min; ISO 527-1
Sax Polymers SAXAMID 126F4MW4 Nylon 6, 40% Glass Fiber and Mineral Reinforced
SAXAMID 126F4MW4 is a 40% glass fibers/ mineral reinforced polyamide 6 injection-molding-grade. It has dimensional stability and high strength.Information provided by SAX Polymers
Tensile Strength 130 MPa
18900 psi
5 mm/min; ISO 527-1
Sax Polymers SAXAMID 126F3 Nylon 6, 15% Glass Fiber
SAXAMID 126F3 is a polyamide 6 injection-molding-grade reinforced with 15% glass fibers.Information provided by SAX Polymers
Tensile Strength 130 MPa

@Thickness >=1.50 mm
18900 psi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 527; IEC/EN 60893-2 5.6
Elektro-Isola Etronit 201M Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: Grade with high mechanical properties but the lowest electrical properties of all Etronit types. Used for mechanical applications.Applications: Dies, topplates and back-up plates for dr..
Tensile Strength 130 MPa
18900 psi
ISO 527
Azoty Tarnow™ Tarnamid® T-27 CF10 Polyamide 6 10% Carbon Fiber - Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..
Tensile Strength 130 MPa
18900 psi
dry; ISO 527
Azoty Tarnow™ Tarnamid® T-27 GF20 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 20% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
Tensile Strength 130 MPa
18900 psi
cond.; ISO 527
Azoty Tarnow™ Tarnamid® T-27 GF30 TF15 Polyamide 6 - Improved Slip Properties
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid..
Tensile Strength 130 MPa
18900 psi
ASTM D638
Solvay Specialty Polymers Veradel® 3330GF Polyethersulfone (PESU)  (Unverified Data**)
Veradel 3330GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime..
Tensile Strength 130 MPa
18900 psi
ASTM D 638
Saint-Gobain Meldin® 1277 Thermoplastic Bearing Material
Meldin 1277 has structural integrity and low deformation. This material also exhibits good electrical insulative properties and dimensional stability.Meldin® 1000 series components are used in app..
Tensile Strength 130 MPa

@Thickness >=1.50 mm
18900 psi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 527; IEC/EN 60893-2 5.6
Elektro-Isola Etronit 201M S Phenolic, Paper Reinforcement, Black, Sheets