Tensile Strength 86.0 MPa
12500 psi
ASTM D-638
PlastiComp Complet® LCF50 - PP Homopolymer Polypropylene, 50% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Tensile Strength 86.0 MPa
12500 psi
at Yield; ISO 527-1/-2
Quadrant EPP Ertalon® 6XAU+ PA 6, heat stabilized, cast (ISO Data)
Ertalon 6 XAU+ is a heat stabilized cast nylon grade with a very dense and highly crystalline structure. Compared with conventional extruded or cast nylons, Ertalon 6 XAU+ offers superior heat agein..
Tensile Strength 86.2 MPa

@Temperature 22.8 °C
12500 psi

@Temperature 73.0 °F
ASTM D638
Quadrant EPP KETRON® MD PEEK, A Metal-Detectable Polyetheretherketone
Tensile Strength 86.2 MPa
12500 psi
ASTM D638
Quadrant EPP Nylatron® GS Nylon, Extruded MoS2 Filled Type 66 (ASTM Product Data Sheet)
Tensile Strength 86.2 MPa
12500 psi
ASTM D638
Solvay Specialty Polymers Radel® R-7625 Polyphenylsulfone (PPSU)
Radel® R-7625 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications that offers improved UV resistance versus Radel® R-7535 and Radel® R-7558. The product ..
Tensile Strength 86.2 MPa
12500 psi
ASTM D638
Teknor Apex Beetle® 140 BH Nylon 66, Glass Bead Reinforced
Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex
Tensile Strength 86.2 MPa
12500 psi
ASTM D638
Teknor Apex Chemlon® 100 Nylon 66, Unreinforced
Features: Basic nylon 66 with internal lubrication. Widely used for automotive, electronic and appliance applications. Processing Method: Injection Molding Forms: Pellets Automotive Specifications: ..
Tensile Strength 86.0 MPa
12500 psi
DIN 53 455
Hippe PI
Wide temperature range for use. High oxidation resistance. UV stability, low coefficient of linear expansion, good strength at high temperatures, resistance against stress cracking.Information pro..
Tensile Strength 86.2 MPa
12500 psi
ASTM D638
Aaron Industries AAROPRENE® MFN 6601 Mineral Filled Nylon 6/6
AAROPRENE® GFN & MFN 6600 Series Reinforced CompoundsColor may be specified.
Tensile Strength 86.2 MPa
12500 psi
ASTM D638
Teknor Apex Chemlon® 109-18 GH Nylon 66, 18% Glass Fiber Reinforced
Notes: High-impact; Reinforced with 18% glass fibers; Highly toughened compound designed to improve practical toughness and ductility Features: Ductile; Good Impact Resistance; Good Toughness; Good ..
Tensile Strength 86.2 MPa

@Temperature 22.8 °C
12500 psi

@Temperature 73.0 °F
ASTM D638
Quadrant EPP Duratron® PAI T7530, Compression Molded Carbon Fiber Reinforced Polyamide-Imide
Tensile Strength 86.2 MPa

@Temperature 22.8 °C
12500 psi

@Temperature 73.0 °F
ASTM D638
Quadrant EPP Duratron® PAI T7530, Compression Molded Carbon Fiber Reinforced Polyamide-Imide
Copyright © lookpolymers.com All Rights Reserved