Polymer Property : Tensile Strength = 12.15 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 12.15 MPa

@Treatment Temp. 120 °C,
Time 3.629e+6 sec
1762 psi

@Treatment Temp. 248 °F,
Time 1008 hour
heat aging; ASTM D573-99
Multibase TPSiV® 3111-70A Thermoplastic Elastomer
TPSiV™ material for injection molding and extrusion applicationsAPPLICATIONS: Solution for appliance, sports and leisure, and construction applications where excellent hydrolysis resistance, high a..