Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 1100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 6.21 - 7.58 MPa
900 - 1100 psi
Compound Property
Arlon 19220R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not be used to w..
Tensile Strength 6.21 - 7.58 MPa
900 - 1100 psi
Compound Property
Arlon 23234R025 0.025" (0.635 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Semi-Cured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications...
Tensile Strength 6.21 - 7.58 MPa
900 - 1100 psi
Compound Property
Arlon 25122R040 0.040" (1.02 mm) Silicone Rubber on Laminated Fluoropolymer Film
Appearance: Red silicone rubber chemically bonded to fluoropolymer filmThis data represents typical values for the production material. The data should not be used to write, or in place of, material..
Tensile Strength 6.21 - 7.58 MPa
900 - 1100 psi
Compound Property
Arlon 25122R060 0.060" (1.52 mm) Silicone Rubber on Laminated Fluoropolymer Film
Appearance: Red silicone rubber chemically bonded to fluoropolymer filmThis data represents typical values for the production material. The data should not be used to write, or in place of, material..
Tensile Strength 6.21 - 7.58 MPa
900 - 1100 psi
Silicone Property
Arlon 27122T125 Cured Silicone Rubber/Skive Tape Laminate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: 5.0 mil Etched Skive Tape bonded to one sideThis data represents typical values for the production material and should not be used as ma..
Tensile Strength 6.21 - 7.58 MPa
900 - 1100 psi
Silicone Property
Arlon 30400R040 0.04" Uncured, Unsupported Silicone Rubber on Release Carrier
Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should..
Tensile Strength 6.21 - 7.58 MPa
900 - 1100 psi
Silicone Property
Arlon 30400R060 0.06" Uncured, Unsupported Silicone Rubber on Release Carrier
Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should..
Tensile Strength 6.21 - 7.58 MPa
900 - 1100 psi
Compound Property
Arlon 51601W015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberProduct Use: Flexible heater insulationAppearance: White silicone gum on fiberglass with polymer release linersThis ..
Tensile Strength 6.21 - 7.58 MPa
900 - 1100 psi
Compound Property
Arlon 75400R045 0.045" (1.14 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info..
Tensile Strength 6.21 - 7.58 MPa
900 - 1100 psi
Compound Property
Arlon 44250R011 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be used to wri..
Copyright © lookpolymers.com All Rights Reserved