Polymer Property : Tensile Strength = 11.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 11.8 MPa
1710 psi
ASTM D412
S&E Specialty Polymers GTPE-2203G1 PVC
Application: RoHS compliant, 105° C, flexible, oil resistant TPE jacketing material with extremely good low temperature properties.Information provided by S&E Specialty Polymers
Tensile Strength 11.8 MPa
1710 psi
ASTM D412
S&E Specialty Polymers TufFlex™ GA-509-75 TPE Compound
Application: A UL listed, sunlight resistant, 75°C rated, UL1277 power limited and control cable jacketing compound for CMX, CL2 and CL3 applications.Information provided by S&E Specialty Polymers
Tensile Strength 11.8 MPa

@Temperature 100 °C,
Time 864000 sec
1710 psi

@Temperature 212 °F,
Time 240 hour
Aged
S&E Specialty Polymers TufFlex™ GA-509-75 TPE Compound
Application: A UL listed, sunlight resistant, 75°C rated, UL1277 power limited and control cable jacketing compound for CMX, CL2 and CL3 applications.Information provided by S&E Specialty Polymers
Tensile Strength >= 11.8 MPa
>= 1710 psi
ASTM D 638
Karina E CAK 85-48/1 Black PVC Compound
Reclaimed PVC compound recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 11.8 MPa
>= 1710 psi
ASTM D 638
Karina TR-700-35/1 Ivory PVC Compound
PVC compound with addition of nitrile rubber, recommended for injection of solesInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 11.8 MPa
>= 1710 psi
ASTM D 638
Karina 752D02/101-AT-IS Yellow PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 11.8 MPa
>= 1710 psi
ASTM D 638
Karina 833D10/184-AY-IS-AS White PVC Compound
PVC compound with additive anti-UV, flame retardant, and fungicide; recommended for extrusion and roll pressed laminated.Information provided by Karina Indústria e Comércio de Plásticos Ltd..
Tensile Strength >= 11.8 MPa
>= 1710 psi
ASTM D 638
Karina E 754-10/426-AT-IS White PVC Compound
White non-toxic PVC compound, recommended for general extrusion.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength 11.8 MPa
1710 psi
Shin-Etsu Silicones LIMSâ„¢ KEG2001-50A/B Elastomer
KEG2001-50 is a very fast cure type liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enou..
Tensile Strength 11.8 MPa
1710 psi
500 in/min; ASTM D638
Teknor Apex Sinvicomp SHE 5600 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Ethylene Oxide Sterilizable Uses: Medical/Healthcare Applications Forms: GranulesInformation Provided by Teknor Apex
Tensile Strength 11.8 MPa
1710 psi
ASTM D412
Dynasol Solprene® 9340 Multi-branched Thermoplastic Rubber (Multi-branched SBS)
Solprene® 9340 is a 66/34 Butadiene-Styrene multi arm copolymer, polymerized in solution process. It has a non-staining FDA approved antioxidant system for food contact applications and it is essen..
Tensile Strength >= 11.8 MPa
>= 1710 psi
After 168 H in Air Oven at 100°C; NBR NM-IEC 60811-1-2
Karina 802D35/1-E-AC-LF Ivory PVC Compound
Heavy metal free and flame retardant PVC compound, recommended for coaxial cables jackets.Information provided by Karina Indústria e Comércio de Plásticos Ltda.