Polymer Property : Tensile Strength = 108 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 108 MPa
15700 psi
ASTM D638
Solvay Specialty Polymers Udel® GF-130 Polysulfone (PSU)  (Unverified Data**)
Udel GF-130, resin is a 30% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resi..
Tensile Strength 108 MPa
15700 psi
ASTM D638
Kolon SPESIN® KP213G20WBL Glass Fiber Reinforced & Weather Resistant PBT Compound Resin
G/F 20% reinforced, weather resistanceApplications: Parts of electric lightInformation provided by API-Kolon.
Tensile Strength 108 MPa
15700 psi
ASTM D638
Kolon SPESIN® KP213G30SB3 Glass Fiber Reinforced PBT Compound Resin
G/F 30% reinforcedApplications: Ignition coil bobbinsInformation provided by API-Kolon.
Tensile Strength 108 MPa
15600 psi
ASTM D638
Gromax PBT 5130-104 30% Glass Fiber Filled
CCP Halogen-free PBT, Black. PBT flame-retarded glass fiber 30% reinforced injection molding gradeCharacteristics:Excellent electrical property Excellent temperature resistance, high heat distortion..
Tensile Strength 108 MPa
15600 psi
50 mm/min; ISO 527-1,-2
Gromax BFG15-DN00N1 Nylon 6 16% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Tensile Strength 108 MPa
15700 psi
ASTM D638
Solvay Specialty Polymers Udel® GF-130 Polysulfone (PSU), Glass Fiber
Udel® GF-130, resin is a 30% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical ..
Tensile Strength 108 MPa
15600 psi
ASTM D638
Samyang Tribit® 1500G20 PBT, Reinforced General Purpose
Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G20 is a reinforced, general purpose gr..
Tensile Strength 108 MPa
15700 psi
ASTM D638
Aaron Industries AAROPRENE® GFPC 5020 Glass Filled Polycarbonate
AAROPRENE® GFPC 5000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified.