Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 74.0 MPa @Thickness 0.0250 mm |
10700 psi @Thickness 0.000984 in |
ASTM D882-02 |
NeXolve CORIN XLS Polyimide Resistant to radiation and atomic oxygen erosion. NeXolve’s CORIN XLSPolyimide is a colorless, clear, organic/inorganic sprayable nanocomposite that is resistant to radiation and atomic oxygen eros.. |
|||
Tensile Strength | 74.0 MPa | 10700 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP Quadrant PC 1000 extruded (ISO Data) Quadrant Engineering Plastic Products is marketing non-UV-stabilized polycarbonate stock shapes under the trade name Quadrant PC 1000. It is a natural, “non-optical” industrial quality (clear, tra.. |
|||
Tensile Strength | 74.0 MPa | 10700 psi | ASTM D638 |
Kolon KOCETAL® GF702 G/F Reinforced Acetal Resin Glass fiber reinforced, improved stiffness. Applications: Products for high stiffness, improved fatigue properties. Information provided by API-Kolon. |
|||
Tensile Strength | 74.0 MPa | 10700 psi | ASTM D638 |
Kolon KOPA® KN333MT30BL Mineral Reinforced Nylon 66 MF reinforcedApplications Cam shaftsInformation provided by API-Kolon. |
|||
Tensile Strength | 74.0 MPa | 10700 psi | ASTM D638 |
KYDEX® FST Fully Compliant Aviation Thermoforming Sheet KYDEX® FST meets all fire, smoke and heat release requirements set forth by the Federal Aviation Regulations 25.853 paragraphs (a) and (d) as well as toxicity requirements for ABD0031, BSS7239 an.. |
|||
Tensile Strength | 73.5 MPa | 10700 psi | ASTM D638 |
Shinkong Synthetic Fibers Shinite® P305G20 PP, 20% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Tensile Strength | 73.5 MPa | 10700 psi | ASTM D638 |
Samyang Trimma® FT6120 I[R] PMMA, Transparent High transparency and high scratch resistance. Stable against weak acids, strong acids, weak alkalis and inorganic salts.Applications: Laptop, Monitor Front Cover - for high flow, high gloss and hi.. |
|||
Tensile Strength | 73.5 MPa | 10700 psi | ASTM D638 |
Samyang Trirex® 3026PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3026PJ is an extrusion grade.Information provided by Samyang. |
|||
Tensile Strength | 73.5 MPa | 10700 psi | ASTM D638 |
Shinkong Synthetic Fibers Shinite® P305G20 PP, 20% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Tensile Strength | 73.5 MPa | 10700 psi | ASTM D638 |
E-Polymers TEKAMID® TA210IR Impact Modified PA66 Resin Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.T-series: Impact modified,.. |
|||
Tensile Strength | 73.5 MPa | 10700 psi | ASTM D638 |
Samyang Trirex® 3026B Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3026B is an extrusion grade.Applications: BottlesInformation provided by Samyang. |
|||
Tensile Strength | 73.5 MPa | 10700 psi | ASTM D638 |
Samyang Trirex® TH3022N Polycarbonate, High Flow Flame Retardancy PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.TH3022N is a high flow, flame retardant grade.Applications: LCD TV, Laptop and Monitor.. |
|||
Tensile Strength | 73.5 MPa | 10700 psi | ASTM D638 |
Gromax CCP PBT 5615-104C 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |