Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 71.0 MPa | 10300 psi | ASTM D-638 |
Plaskolite Optix® CA - 75 HID General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Tensile Strength | 71.0 MPa | 10300 psi | ASTM D-638 |
Plaskolite Optix® CA - 75 LL General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Tensile Strength | 71.0 MPa | 10300 psi | ASTM D-638 |
Plaskolite Optix® CA - 75 OG General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Tensile Strength | 71.0 MPa | 10300 psi | ASTM D-638 |
Plaskolite Optix® CA - 75 UVA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Tensile Strength | 71.0 MPa | 10300 psi | ASTM D-638 |
Plaskolite Optix® CA - 75 UVT General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Tensile Strength | 71.0 MPa | 10300 psi | ASTM D-638 |
Plaskolite West Optix® CA - 75 HID General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Tensile Strength | 71.0 MPa | 10300 psi | ASTM D-638 |
Plaskolite West Optix® CA - 75 UVA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Tensile Strength | 71.0 MPa | 10300 psi | ASTM D-638 |
Plaskolite West Optix® CP - 75 HID General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Tensile Strength | 71.0 MPa | 10300 psi | ASTM D-638 |
Plaskolite West Optix® CA - 75 LL General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Tensile Strength | 71.0 MPa | 10300 psi | ASTM D-638 |
Plaskolite West Optix® CP - 75 UVA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Tensile Strength | 71.0 MPa | 10300 psi | |
Henkel Hysol Benzoxazine 99110 Infusion Resin One-part Infusion resin for RTM & VARTM processing. Low viscosity, high hot-wet properties and very good resistance against flame, smoke and toxicity. |
|||
Tensile Strength | 71.0 MPa | 10300 psi | DIN EN ISO 527 |
Wolf Kunststoff ZEDEX® ZX-410V7T A4T Polymer Alloy, Fiber Reinforced, Friction Modified Main Characteristics: Fiber-reinforced; Friction-modified; Very high stiffness (higher than that of fiber-reinforced PEEK); Very low thermal expansion coefficient; Low friction; High wear resistance.. |
|||
Tensile Strength | 71.0 MPa | 10300 psi | ASTM D412 |
Lubrizol Estane® ETE 55DS3 Thermoplastic Polyurethane, Easy-to-Extrude Type: Estane® ETE 55DS3 is a 55D aromatic polyester-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, .. |
|||
Tensile Strength | 71.0 MPa | 10300 psi | Machine; ASTM D882 |
Arlon CuClad 233 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate CuClad 233 uses a medium fiberglass/PTFE ratio to balance lower dielectric constant and improved dissipation factor without sacrificing mechanical properties.Cross Plied Woven Fiberglass, alternatin.. |
|||
Tensile Strength | 71.0 MPa | 10300 psi | ASTM D-638 |
Plaskolite Optix® CP - 75 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Tensile Strength | 71.0 MPa | 10300 psi | ASTM D-638 |
Plaskolite Optix® CP - 75 HID General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Tensile Strength | 71.0 MPa | 10300 psi | ASTM D-638 |
Plaskolite Optix® CP - 75 UVA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Tensile Strength | 71.0 MPa | 10300 psi | ASTM D-638 |
Plaskolite West Optix® CA - 75 OG General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Tensile Strength | 71.0 MPa | 10300 psi | ASTM D-638 |
Plaskolite West Optix® CA - 75 UVT General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Tensile Strength | 71.0 MPa | 10300 psi | ASTM D-638 |
Plaskolite West Optix® CP - 75 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |