Polymer Property : Tensile Strength = 102 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 102 MPa
14800 psi
at Yield; ISO 527-1/-2
Quadrant EPP Techtron® PPS unfilled, extruded (ISO Data)
This unfilled polyphenylene sulfide based material is ideal for structural applications in corrosive environments or as a PEEK replacement at less demanding temperatures. Very good dimensional stabi..
Tensile Strength 102 MPa
14800 psi
ASTM D638
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over a b..
Tensile Strength 102 MPa
14800 psi
ASTM D638
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA), 22% Mineral
Amodel® A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over..
Tensile Strength 102 MPa
14800 psi
ASTM D638
Shinkong Synthetic Fibers Shinite® F202G30 PBT, 30% Glass Filled, Fire Retardant, Halogen Free
Information from Shinkong Synthetic Fibers Corp.
Tensile Strength 102 MPa
14800 psi
ASTM D638
Shinkong Synthetic Fibers Shinite® F202G30 PBT, 30% Glass Filled, Fire Retardant, Halogen Free
Information from Shinkong Synthetic Fibers Corp.
Tensile Strength 102 MPa

@Strain 8.00 %,
Temperature 0.000 °C
14800 psi

@Strain 8.00 %,
Temperature 32.0 °F
50 mm/min; ISO 527-2
BASF Elastollan R 3000 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Tensile Strength 102 MPa
14800 psi
ASTM D638
Aaron Industries AAROPRENE® GFN 6613 Glass Filled Nylon 6/6
AAROPRENE® GFN & MFN 6600 Series Reinforced CompoundsColor may be specified.