Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1.20 MPa | 174 psi | |
Shin-Etsu Silicones KE-1867 Silicone, RTV Adhesive/Sealant Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tensile Strength | 1.20 MPa @Strain 20.0 % |
174 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan S 70 AWH TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | >= 1.20 MPa | >= 174 psi | in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® R63.80 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable.. |
|||
Tensile Strength | >= 1.20 MPa | >= 174 psi | in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® R82.60 High Performance Structural Foam AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, ver.. |
|||
Tensile Strength | >= 1.20 MPa | >= 174 psi | perpendicular to plane; ASTM C297 |
3A Composites Core Materials AIREX® T90.60 Easy Processing Structural FST Foam AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu.. |