Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 0.700 MPa | 102 psi | average; in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® C70.40 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |