Mechanical Properties Metric English Comments
Tensile Strength 0.375 MPa
54.4 psi
ISO 7214 1998
Zotefoams Plastazote® LD30SD Static Dissipative Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Tensile Strength 0.375 MPa
54.4 psi
ISO 7214 1998
Zotefoams Plastazote® LD29 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..