Polymer Property : Tear Strength, Total = 5.62 lb (f) Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength, Total 25.0 N
5.62 lb (f)
Initial in TD; ASTM D1004
DuPont™ Nomex® E56 Paper, 10 mil Nominal Thickness
Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as..
Tear Strength, Total 25.0 N
5.62 lb (f)
Initial in MD; ASTM D1004
DuPont™ Nomex® E56 Paper, 5 mil Nominal Thickness
Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as..