Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength, Total | 38.0 N | 8.54 lb (f) | Initial in TD; ASTM D1004 |
DuPont™ Nomex® 414 Paper, 10 mil Nominal Thickness Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand.. |
|||
Tear Strength, Total | 38.0 N | 8.54 lb (f) | Initial in MD; ASTM D1004 |
DuPont™ Nomex® 418 Paper, 14 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Tear Strength, Total | 38.0 N | 8.54 lb (f) | Initial in MD; ASTM D1004 |
DuPont™ Nomex® E56 Paper, 7 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |