Polymer Property : Tear Strength, Total = 13.0 N Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength, Total 13.0 N
2.92 lb (f)
Initial in MD; ASTM D1004
DuPont™ Nomex® 411 Paper, 10 mil Nominal Thickness
Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil..
Tear Strength, Total 13.0 N
2.92 lb (f)
Initial in TD; ASTM D1004
DuPont™ Nomex® E56 Paper, 5 mil Nominal Thickness
Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as..