Polymer Property : Tensile Impact = 50.2 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact 50.2 J/cm
94.0 ft-lb/in
ASTM D1822
Westlake Plastics Imidex Thermoplastic Polyimide
Made from Aurum® resin. Applications include electronics, acoustics, composites, wire/cable insulation, adhesive film, and washers/gaskets. It will not melt unto itself, is thermoformable, has hi..