Chemical Properties | Metric | English | Comments |
---|---|---|---|
Ionic Impurities - Fe (Iron) | <= 80 ppm | <= 80 ppm | |
Solvay Sulfuric Acid 70% Technical Grade Description: Sulfuric Acid is a colorless, clear to hazy, odorless, oily-looking liquid. It is very corrosive. Complies with Federal Specification A-A-55828, Type I, Class 2 and Type II, Class 2.For.. |
|||
Ionic Impurities - Fe (Iron) | <= 80 ppm | <= 80 ppm | |
Solvay Sulfuric Acid 78% Technical Grade Description: Sulfuric Acid is a colorless, clear to hazy, odorless, oily-looking liquid. It is very corrosive. Complies with Federal Specification A-A-55828, Type I, Class 2 and Type II, Class 2.For.. |
|||
Ionic Impurities - Fe (Iron) | <= 80 ppm | <= 80 ppm | |
Solvay Sulfuric Acid 93% Technical Grade Description Sulfuric Acid is a colorless, clear to hazy, odorless, oily-looking liquid. It is very corrosive. Complies with Federal Specification A-A-55828, Type I, Class 2 and Type II, Class 2.Form.. |
|||
Ionic Impurities - Fe (Iron) | <= 80 ppm | <= 80 ppm | |
Solvay Sulfuric Acid 96% Technical Grade Description Sulfuric Acid is a colorless, clear to hazy, odorless, oily-looking liquid. It is very corrosive. Complies with Federal Specification A-A-55828, Type I, Class 2 and Type II, Class 2.Form.. |
|||
Ionic Impurities - Fe (Iron) | <= 80 ppm | <= 80 ppm | |
Solvay Sulfuric Acid 98% Technical Grade Description sulfuric Acid is a colorless, clear to hazy, odorless, oily-looking liquid. It is very corrosive. Complies with Federal Specification A-A-55828, Type I, Class 2 and Type II, Class 2.Form.. |
|||
Ionic Impurities - Fe (Iron) | <= 80 ppm | <= 80 ppm | |
Solvay Sulfuric Acid 99% Technical Grade Description sulfuric Acid is a colorless, clear to hazy, odorless, oily-looking liquid. It is very corrosive. Complies with Federal Specification A-A-55828, Type I, Class 2 and Type II, Class 2.Form.. |