Polymer Property : Linear Mold Shrinkage, Flow = 0.0028 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0028 cm/cm

@Time 86400 sec
0.0028 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP RFN16S PA 66
LNP LUBRICOMP* RFN16S is a compound based on Nylon 66 resin containing 30% Glass Fiber, 5% MOS2. Added features of this material include: Heat Stabilized, Wear Resistant.
Linear Mold Shrinkage, Flow 0.0028 cm/cm

@Time 86400 sec
0.0028 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP RFN16SXZ PA 66
LNP LUBRICOMP* RFN16SXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber, 5% MOS2. Added features of this material include: Heat Stabilized, Wear Resistant.
Linear Mold Shrinkage, Flow 0.0028 cm/cm

@Time 86400 sec
0.0028 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Lubricomp ZFL36CCX PPE+PS
LNP LUBRICOMP* ZFL36CCX is a compound based on PPE+PS Blend resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for..
Linear Mold Shrinkage, Flow 0.0028 cm/cm

@Time 86400 sec
0.0028 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DX06500 PC (Asia Pacific)
LNP* Stat-kon* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0028 - 0.0031 cm/cm

@Time 86400 sec
0.0028 - 0.0031 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK
LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive
Linear Mold Shrinkage, Flow 0.0028 - 0.0031 cm/cm

@Time 86400 sec
0.0028 - 0.0031 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK (Asia Pacific)
LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Flow 0.0028 cm/cm

@Time 86400 sec
0.0028 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP RF008XXZ PA 66
LNP THERMOCOMP* RF008XXZ is a compound based on Nylon 66 resin containing 40% Glass Fiber.
Linear Mold Shrinkage, Flow 0.0028 cm/cm

@Time 86400 sec
0.0028 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP ZF0049 PPE+PS (Asia Pacific)
LNP* Thermocomp* ZF0049 is a compound based on PPE+PS Blend resin containing Flame Retardant. Added features of this material include: Flame Retardant.
Linear Mold Shrinkage, Flow 0.0028 cm/cm

@Time 86400 sec
0.0028 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DX06500 PC
LNP* STAT-KON* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive, Wear Resistant, Easy ..
Linear Mold Shrinkage, Flow 0.0028 cm/cm

@Time 86400 sec
0.0028 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-LOY PF306 PA 6
LNP* STAT-LOY* PF306 is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added feature of this grade includes: Antistat.
Linear Mold Shrinkage, Flow 0.0028 cm/cm

@Time 86400 sec
0.0028 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP ZF0049 PPE+PS
LNP* THERMOCOMP* ZF0049 is a compound based on PPE+PS resin containing 20% Glass Fiber. Added feature of this material is: Flame Retardant.