Polymer Property : Linear Mold Shrinkage, Flow = 0.00050 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.00050 cm/cm

@Time 86400 sec
0.00050 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-kon DEL339XC PC
LNP STAT-KON* DEL339XC is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE, Flame Retardant. Added features of this material include: Electrically Conductive.This data was supp..
Linear Mold Shrinkage, Flow 0.00050 cm/cm

@Time 86400 sec
0.00050 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DX99873C PC
LNP STAT-KON* DX99872C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00050 - 0.0030 cm/cm

@Time 86400 sec
0.00050 - 0.0030 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON EE005E PEI
LNP STAT-KON* EE005E is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00050 - 0.0030 cm/cm

@Time 86400 sec
0.00050 - 0.0030 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON EE005E PEI (Asia Pacific)
LNP STAT-KON* EE005E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Flow 0.00050 cm/cm

@Time 86400 sec
0.00050 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK
LNP* THERMOCOMP* LC008E is a compound based on Polyetheretherketone resin containing 40% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00050 cm/cm

@Time 86400 sec
0.00050 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK (Asia Pacific)
LNP* Thermocomp* LC008E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00050 cm/cm

@Time 86400 sec
0.00050 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-kon DEL339XC PC (Asia Pacific)
LNP STAT-KON* DEL339XC is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was supp..
Linear Mold Shrinkage, Flow 0.00050 - 0.0010 cm/cm

@Time 86400 sec
0.00050 - 0.0010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP VERTON UX03320 PPA
LNP* VERTON* UX03320 is a compound based on Polyphthalamide resin containing proprietary fillers. Added feature of this grade is: Structural.
Linear Mold Shrinkage, Flow 0.00050 - 0.0010 cm/cm

@Time 86400 sec
0.00050 - 0.0010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Europe-Africa-Middle East)
VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass.
Linear Mold Shrinkage, Flow 0.00050 - 0.0010 cm/cm

@Time 86400 sec
0.00050 - 0.0010 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Asia Pacific)
VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass.