Polymer Property : Vapor Pressure = 69.2 torr Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Vapor Pressure 0.0923 bar

@Temperature 0.000 °C
69.2 torr

@Temperature 32.0 °F
LG Chemical Acetone
Overview: Acetone is the raw material of MMA(Methyl Metha Acrylate), BPA, ascorbic acid (Vitamin C), etc. In addition, acetone is widely used as solvents for synthetic resins, rubber, oil paper and ..