Polymer Property : Vapor Pressure = 15.0 torr Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Vapor Pressure 0.0200 bar

@Temperature 193 °C
15.0 torr

@Temperature 380 °F
Paratherm Corporation Paratherm™ GLT™ Heat Transfer Fluid
Paratherm GLT™ Heat Transfer Fluid is an alkylated aromatic based heat transfer fluid formulated for closed loop liquid phase heating systems to 550°F using fired heaters and to 575°F in waste-he..
Vapor Pressure 0.0201 bar

@Temperature 120 °C
15.0 torr

@Temperature 248 °F
Solvay Chemicals Glycerol alpha monochlorohydrin
Viscous liquid used as chemical intermediate.EINECS Number: 202-492-4/CAS Number: 96-24-2/UN number: 2689Information provided by Solvay